12R11
Main mechanical properties
expressed in MPa (nominal values at 20°C; tolerance ±100 MPa)
| Material | Breaking load Rm | Yield strength Rp0.2% | Elastic limit 0.01% | Module E | Module G | Stretching | Maximum serving temperature |
|---|---|---|---|---|---|---|---|
| ALLEIMA/SANDVIK 12R11 | 1225 | 1100 | 650 | 185.000 | 70.000 | A11.3 15% | 250 °C |
| ALLEIMA/SANDVIK 12R11 | 1500 | 1375 | 800 | 182.000 | 70.000 | A11.3 8% | 250 °C |
| ALLEIMA/SANDVIK 12R11 | 1700 | 1625 | 950 | 180.000 | 69.000 | A11.3 1.5% | 250 °C |
Description and uses
Austenitic chromium-nickel stainless steel. Multipurpose, with good mechanical properties, its characteristics meet most standard requirements for corrosion resistance, mechanical resistance, fatigue resistance, and relaxation.
Check availability (subject to prior sale)
For more information, contact us now!